Quick Answer

After a 30 or 50 grit metal bond, start resin at 50 or 100 grit, not 200. The first resin step must remove the metal-bond scratch pattern. If the metal bond left deep grooves, use a copper-bond transition pad before the 50 grit resin.

Why the Jump Matters

Metal-bond diamonds cut deep and fast. Resin pads cut shallow and fine. If you jump from a 30 grit metal bond to a 200 grit resin, the resin cannot remove the deep scratches; it only polishes their peaks. The floor looks shiny but the scratch pattern is still there.

The correct first resin grit depends on the metal-bond grit and the surface. A 30 grit metal bond usually needs a 50 grit resin; a 50 grit metal bond can start at 100 grit resin.

When to Use a Transition Pad

A copper-bond transition pad cuts like a fine metal bond but leaves a surface that resin can refine. Use it when the metal bond leaves visible grooves, when the concrete is hard and the resin loads, or when the floor has a dense aggregate that the resin cannot cut.

Do not use a transition pad to skip the first resin step. It prepares the surface; it does not replace the sequence.

Checking the Scratch

Stop the machine and look at the floor under raking light. If the metal-bond scratches cross the resin scratches, repeat the resin step. If the surface is uniform, move to the next grit.

Frequently Asked Questions

Q: Can I go from 30 metal to 100 resin?

A: Yes, if the metal bond was fully worn and the floor is flat. Check the scratch pattern before continuing.

Q: Do I need a transition pad on soft concrete?

A: Usually not. Soft concrete cuts easily with resin. Use transition on hard, dense floors.

Q: Why does the resin pad load?

A: The metal-bond scratches are too deep or the resin grit is too fine. Start coarser or use a transition pad.

Conclusion

Let the scratch pattern decide the first resin grit. A copper-bond transition pad bridges hard floors; a resin floor polishing pad carries the main sequence.

Products used in this guide

Need this tool for your job?

MOQ 1 · 7–30 days by order quantity · FOB & CIF · free sample on request

Get a factory quote

Share this article

Author & Manufacturer

Written and reviewed by JOY TECH - an SGS & BV audited, CE/RoHS certified diamond tools manufacturer founded in 2004, exporting to 50+ countries.

Quality & Compliance

Our factory and quality management system are audited by SGS and Bureau Veritas. Products meet CE/RoHS requirements and every piece is 100% inspected before packing.

Verified Certificates

  • • SGS Audited Supplier — Report No. QIP-ASI227442 & QIP-ASR247051
  • • Bureau Veritas Verified — Report No. MIC-ASR257059
  • • CE & RoHS Certificate of Conformity — No. CS240925001HRZ

Request a Factory Quote

Average response time: under 24 hours

Or WhatsApp: +86 185 5928 2197 · [email protected]

FAQ

GET A QUOTEWhatsApp