Skip to content
JOY TECH — Concrete Polishing Tools logo

Removing Mastic With PCD vs Diamond Grinding

Scroll

Removing Mastic With PCD vs Diamond Grinding

2026-11-19•JTJOY TECH Engineering Team
Removing Mastic With PCD vs Diamond Grinding

Quick Answer

Use PCD for thick mastic, epoxy and glue. Use diamond grinding for the thin residue left after the bulk is removed. PCD cuts the coating without loading; diamond cuts the concrete and prepares the surface.

What PCD Does

PCD is polycrystalline diamond. It is a flat, hard cutter that shaves coating off the surface. It works on mastic, adhesive, epoxy and paint. It does not cut concrete deeply, so it leaves the profile almost unchanged.

PCD is aggressive. Keep the machine moving and use a dust shroud. A PCD tool held in one spot can gouge the concrete.

What Diamond Does

A diamond grinding block cuts the concrete and removes the last layer of coating. It is used after PCD, or on thin coatings that PCD would skip over. Diamond grinding also opens the surface for the next step.

Diamond grinding on thick mastic will load the segment and smear the coating. That is why PCD comes first.

Sequence

  • Remove bulk mastic with PCD.
  • Remove residue with a 16 or 20 grit diamond block.
  • Grind to the required profile with 30 or 50 grit.
  • Vacuum and inspect before applying a new coating.

Frequently Asked Questions

Q: Can I use PCD on thin glue?

A: It may be too aggressive. Use diamond grinding for thin residue.

Q: Why does the diamond block load?

A: The coating is too thick or the bond is too soft. Remove more with PCD first.

Q: Does PCD leave a smooth surface?

A: No. It leaves a shaved surface that still needs diamond grinding before a new finish.

Conclusion

PCD removes the bulk; diamond prepares the concrete. A WerkMaster PCD tool is a strong first cut; an HTC PCD tool suits epoxy and glue removal.

Products used in this guide

Need this tool for your job?

MOQ 1 · 7–30 days by order quantity · FOB & CIF · free sample on request

Get a factory quote

Share this article

Author & Manufacturer

Written and reviewed by JOY TECH - an SGS & BV audited, CE/RoHS certified diamond tools manufacturer founded in 2004, exporting to 50+ countries.

Quality & Compliance

Our factory and quality management system are audited by SGS and Bureau Veritas. Products meet CE/RoHS requirements and every piece is 100% inspected before packing.

Verified Certificates

  • • SGS Audited Supplier — Report No. QIP-ASI227442 & QIP-ASR247051
  • • Bureau Veritas Verified — Report No. MIC-ASR257059
  • • CE & RoHS Certificate of Conformity — No. CS240925001HRZ

Request a Factory Quote

Average response time: under 24 hours

Or WhatsApp: +86 185 5928 2197 · [email protected]

FAQ

GET A QUOTEWhatsApp