An outdoor recycling yard cuts old, abrasive, steel-free concrete floors; the operator tracked metres cut per blade.

The job

Highly abrasive old concrete with no steel to guide the blade, and no water supply beyond a hose line.

What we supplied

A harder bond and lower segment height to resist abrasion, trialled on the same 7.5 kW saw.

Result

Stable cutting at about 12 m² per blade; the honest feedback was used to tune the next batch toward longer life.

What the customer said

“They run very well in old concrete without steel — about 12 m² per blade, though it could be a little more.”

— Daniel · Verified purchase · message on file · 2024-08-12 · 4/5

Customer names are published with the customer's permission. Quantities, metres and tool life are as reported by the customer, not independently audited.