Skip to content
JOY TECH — Concrete Polishing Tools logo

Sandstone cutting in Poland — a full segment life

Scroll

Sandstone cutting in Poland — a full segment life

A Polish stone fabricator cut abrasive sandstone blocks with a 350 mm blade until the segments were used up.

The job

Abrasive sandstone wears segments quickly, so cost per cut depends on how evenly the bond wears.

What we supplied

Segment bond and diamond grade selected for abrasive sandstone, with a 20-blade trial order shipped by air.

Result

The blade ran to full segment consumption with no quality remarks, and the customer held a follow-up order pending demand.

What the customer said

“The blade ran until the segments were fully consumed, with no remarks on cutting quality.”

— Adam · Verified purchase · message on file · 2026-07-31 · 4/5

Customer names are published with the customer's permission. Quantities, metres and tool life are as reported by the customer, not independently audited.