Average response time: under 24 hours

Most coating problems are prep problems in disguise. Clean the floor, then run a high-speed burnisher (1500+ rotations per minute) with a white pad, or a floor equipment with a beige pad, using a dry burnish pass. Yes — you can burnish an epoxy resin-coated floor to make it shinier.
For machine-matched tooling, browse our Diamond Resin Polishing Pads for Concrete & Terrazzo... range.Key factors in coating work.
This is the step that decides whether the coating lasts.
What causes it.
Getting prep wrong here shows up later as peeling or delamination.
The details that matter.
White (100% synthetic) pads are the standard for final mirror finish on epoxy resin.
Most coating warranties start and end with the surface profile.
A: For most jobs, The coating layer may be old, scratched, or the burnisher speed too low. Deep scratch marks require recoating; surface dullness requires a clean white pad at 1500+ rotations per minute.
A: In short, Yes, a low-speed buffer (300–500 rotations per minute) with a beige pad removes scuffs, but a high-speed burnisher gives the real mirror finish.
A: The practical answer is, Weekly to monthly for commercial floors, depending on traffic. Light fine dust-mopping daily extends the mirror finish between burnishes.
Looking for the right tool? Check our Diamond Resin Floor Polishing Pads. Looking for the right tool? Check our 8 Triangles Diamond Resin Floor Polishing Pads.Do the prep thoroughly and the coating system performs as designed. Epoxy resin floors reflectivity with a simple burnish routine: clean, dry, and burnish with a white pad at high speed.
Written and reviewed by JOY TECH - an SGS & BV audited, CE/RoHS certified diamond tools manufacturer founded in 2004, exporting to 50+ countries.
Our factory and quality management system are audited by SGS and Bureau Veritas. Products meet CE/RoHS requirements and every piece is 100% inspected before packing.
Verified Certificates