Coatings only bond as well as the surface they sit on. To strip 2-3 mm of old epoxy resin, polyurethane or paint build-up, use PCD tooling at low speed in shallow, overlapping passes. Strip thick build-up with PCD tooling at low speed in shallow, overlapping passes — do not force the full 2-3 mm depth in one cut.
For machine-matched tooling, browse our Husqvarna Redi Lock PCD Diamond Grinding Disc for Ep... range.The details that matter.
Most coating warranties start and end with the surface profile.
Key factors in coating work.
After stripping, follow with 30/46 metal-bond abrading to strip the last coating layer film and profile the concrete.
This is the step that decides whether the coating lasts.
A: In short, Only when the slab is already even and you are refining. On coarse or ground-new concrete, skipping leaves a scratch mark pattern finer pads cannot resolve.
A: The practical answer is, When segments glaze and stop sawing, the bond is too hard; if they wear level in under half a set, it is too soft. Match bond to concrete hardness.
A: For most jobs, Dry abrading with a HEPA industrial vacuum is standard on glossy concrete projects; wet abrading is mostly used for stone and edge work to control fine dust and heat.
A: In short, Change the whole set together once segment height drops by half or the cut rate slows. Mixing new and worn plates causes uneven scratch mark patterns.
Looking for the right tool? Check our Triple PCD Husqvarna Diamond Grinding Disc for Epoxy.... Looking for the right tool? Check our Triple PCD with Single Round Segment Diamond Grindin....The surface profile is the whole game - fix it before the coating goes on. Selecting the right bond, grit stage and technique for your concrete project saves tooling investment and avoids rework.
Written and reviewed by JOY TECH - an SGS & BV audited, CE/RoHS certified diamond tools manufacturer founded in 2004, exporting to 50+ countries.
Our factory and quality management system are audited by SGS and Bureau Veritas. Products meet CE/RoHS requirements and every piece is 100% inspected before packing.
Verified Certificates