Average response time: under 24 hours

Coating failure almost always starts with surface preparation. Strip a commercial epoxy resin floor in two passes: PCD tooling to shave off the bulk coating layer, then a 30/46 metal-bond disc to clean up the residue and profile the slab. On a 500 m2 retail floor, budget one full workday with a 700-800 mm ride-on grinder and two operators.
For machine-matched tooling, browse our WerkMaster PCD Tooling for Coating Removal range.What causes it.
After the bulk is gone, a light metal-bond pass removes the film residue and opens the concrete.
Getting prep wrong here shows up later as peeling or delamination.
The details that matter.
Browse the full range in our concrete abrading discs category.
Most coating warranties start and end with the surface profile.
Key factors in coating work.
This is the step that decides whether the coating lasts.
What causes it.
Getting prep wrong here shows up later as peeling or delamination.
A: The practical answer is, Up to about 2 mm of epoxy resin. Thicker build-ups require multiple passes.
A: For most jobs, Yes. PCD leaves a deep scratch mark and a light resin film. Metal-bond cleanup gives the CSP profile the new coating layer requires.
A: In short, For small areas, yes. For 500 m2 commercial work, abrading is faster and leaves a more suitable profile.
Looking for the right tool? Check our WerkMaster PCD Tooling for Epoxy Floor Removing. Looking for the right tool? Check our Husqvarna Piranha PCD Tool for Concrete Floor Coatin....The surface profile is the whole game - fix it before the coating goes on. Commercial epoxy resin stripping is a two-tool project: PCD for the bulk, metal-bonded matrix for the profile.